International code name |
SK35 | SK36 | SK37 | SK38 | SK40 |
Al2O3/% |
≥48 | ≥55 | ≥65 | ≥75 | ≥80 |
Fe2O3/% |
≤2 | ≤2 | ≤2 | ≤2 | ≤2 |
Refractoriness |
≥1750 °C | ≥1770 °C | ≥1790 °C | ≥1790 °C | ≥1790 °C |
Apparent porosity |
≤22% | ≤22% | ≤23% | ≤23% | ≤21% |
Cold crushing strength |
≥39Mpa | ≥44Mpa | ≥49Mpa | ≥54Mpa | ≥65Mpa |
Refractoriness under load (0.2MPa) |
≥1420 °C | ≥1470°C | ≥1500 °C | ≥1520 °C | ≥1530 °C |
Reheating Linear Change (1500°C 2h) % | +0.1~ -0.4 *1450°C |
+0.1~ -0.4 | +0.1~ -0.4 |
|